Aladdin Welding Products Inc.

White Metal Handbook...
Brazing Aluminum with Aladdin #31 3-in-1 Rod

Welding Zinc-Base Metals with Aladdin #31 3-in-1 Rod

Soldering Aluminum with Aladdin #33 Low Melt Rod

Soldering Aluminum with Aladdin #604

Soft SilverSoldering with Aladdin #450

Repairing a Propeller
About Us Products Catalog Solder Book White Metal Handbook Testimonials Contact Us
Brazing Aluminum with Aladdin #31 3-in-1 Rod
Brush surface to be repaired thoroughly under heat to break up surface oxide.
Heat the metal hot enough to flow the rod without the aid of the flame, thoroughly tinning the surface.
Brush tinned surface under heat, thoroughly filling open pores. This constitutes welding without fusion.
With sides thoroughly tinned, flow enough rod to fill the Vee. Be sure the filler metal fuses with the tinned surface without melting the base metal.

  Aladdin Welding Products, Inc.   1300 Burton St. SE   P.O. Box 49510-7188   Grand Rapids, MI 49507